• Gnc30 1.2V 30ah 48V System
  • Gnc30 1.2V 30ah 48V System
  • Gnc30 1.2V 30ah 48V System
  • Gnc30 1.2V 30ah 48V System

Gnc30 1.2V 30ah 48V System

Type: Ni-CD Battery
Usage: Car, Electric Power, Lighting
Nominal Voltage: 1.2V
Discharge Rate: Ultrahigh Discharge Rate
Shape: Square Battery
Electrolyte: Alkaline
Samples:
US$ 50/Piece 1 Piece(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2016

Suppliers with verified business licenses

Manufacturer/Factory

Basic Info.

Model NO.
GNC30
Installation
Fixed
Rechargeable
Chargeable
Transport Package
Plywood Case
Trademark
Hengming or ODM
Origin
Made in China
HS Code
8507300000

Product Description

1.  Benefits of ni cd  battery  as below : 

  • Excellent charging efficiency and smooth discharge voltage
  • High reliability without sudden death
  • Ability to withstand ultra-high and ultra-low environmental temperatures
  • Withstand physical and mechanical abuses
  • Exceptionally long & reliable service life
  • Pollution-free,total green energy
  • low Self-discharging
  • No emission of corrosive gases, Safe from flame & explosion
  • Pollution-free and excellent mechanical strength
  • Convenient for installation and low maintenance
  • Availability to design and manufacture other model according to user's requirements 

    2. The Discharge table : 

     

    Rate constant of current(A) Final voltage(V) Low rate Medium rate High rate
    0.2C5 1.0 5h 5h 5h
    1 C5 1.0 / 40min 50min
    5 C5 0.8 / / 4min

    3. roubles and trouble shootings

    Troubles Causes Trouble shootings
     
     
     
     
    The capacity of the battery decreases
    1.The electrolyte has been used for a long time and the carbonate content in it is too high. Replace the electrolyte
    2.The electrolyte is un-properly used. Replace the electrolyte
    3.The electrolyte isn't enough,and the level of the electrolyte is below the top of the plates. See Table 5
    4.Harmful impurities contained in the electrolyte is too high. Replace the electrolyte
    5.The charge/discharge method is not correct. See the 5.2 and 6
    6.Short-circuit or slight-short circuit in the cell Replace the short-circuit cell.
    7.Short-circuit or slight-short circuit occurs out of the cell. Keep the cells in a dry temperature
    8.The instruments used is not correct. Check and rectify the ampere meter and voltmeter.
    Voltage is uncorrect 1.The inner circuit of the cell is short or cut,the electrolyte has been run out. Clean the cell, or change the electrolyte
    2.The out circuit of the battery is short or cut. Keep the cell dry,and check
    3.Contact fault Check and repair
    Bubbles appear in the inside of the cell The electrolyte contains organic impurites Replace the electrolyte
    The cell container swells 1.The positive plate swells. If necessary,change the cell.
    2.The vent is blocked up. Clean with hot water or replace it.


     

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now

You Might Also Like

Diamond Member Since 2016

Suppliers with verified business licenses

Manufacturer/Factory
Management System Certification
ISO9001:2015, ISO14001:2015, ISO45001:2018 Certificate
International Commercial Terms(Incoterms)
FOB, CIF, CFR